PCB Surface Finishes, Defined for the Application

Complete engineering guidance for solderable, contact, bonding, RF and functional surface finishes—from lead-free HASL and OSP to ENIG, ENEPIG, nickel-free EPIG, immersion silver, immersion tin and selective metal systems.

Prototype to volume · DFM review · Mixed and selective finishes

Confirmed EPIG
Pd 1–5 µin · Au 1–5 µin
16+finish systems and variants
ENIG 520 × 800 mmlisted maximum size
HASL 520 × 650 mmlisted maximum size
Hard gold 450 × 500 mmlisted maximum size
DFM + CAM reviewdrawing-based release

Surface protection and solderability

Why the finish matters

A PCB surface finish protects exposed copper from oxidation and creates a dependable interface for soldering, wire bonding, edge connectors and electrical contacts. Selection depends on pitch, assembly process, storage, environment, reliability and cost.

One PCB may use different finishes in different areas. Solderable pads, connector contacts, wire-bonding surfaces and carbon contacts must be reviewed against the released fabrication drawing.

01 · SOLDERABLE

Flat assembly surfaces

For SMT, BGA, QFN and fine-pitch assembly.

ENIGOSPLF-HASLImAg
02 · CONTACT

Wear-resistant surfaces

For gold fingers, connectors, insertion and repeated mating.

Hard GoldSelective GoldNi/Au
03 · ADVANCED

Bonding and RF

For wire bonding, mixed technology, high frequency and nickel-sensitive designs.

ENEPIGEPIGSoft Gold
04 · FUNCTIONAL

Conductive coatings

For keypads, switches and special conductive features.

Carbon InkSilver Paste

Layer logic

Define the metal stack, treated area and thickness

Finish names alone are not complete specifications. Define whether deposition is chemical or electrolytic, whether treatment is full-board or selective, and the target thickness for every functional zone.

Nickel-free EPIG: the nickel barrier is intentionally omitted. KKPCB capability is Pd 1–5 µin (0.025–0.127 µm) and Au 1–5 µin (0.025–0.127 µm), subject to engineering confirmation.
Au · contact or solderability
Pd · barrier or bonding
Ni · diffusion barrier
Cu · PCB pad base

Complete finish reference

Surface finish options and practical use

Core solderable finishes, advanced metal systems, electrolytic deposits, selective processes and functional conductive coatings are listed below. Similar names are identified without double-counting aliases.

Finish System / abbreviation Typical use Engineering note
Lead-Free HASL Hot-air solder leveling / LF-HASL General RoHS assembly Robust and economical; less flat for the finest pitch.
Leaded HASL Hot-air solder leveling / HASL Legacy or specified industrial products Use only when drawing, destination market and regulations allow it.
OSP Organic solderability preservative Fine-pitch SMT and cost-sensitive builds Flat and economical; storage and multiple thermal cycles need review.
Immersion Silver ImAg / IS Fine pitch, RF and high-frequency boards Flat solderable surface; protect from sulfur and contamination.
Immersion Tin ImSn / IT Fine-pitch soldering and selected assembly Shorter storage window and oxidation sensitivity require controlled handling.
ENIG Electroless Nickel Immersion Gold / NiAu BGA, QFN, fine pitch and general SMT Flat pad with nickel barrier; confirm Ni and Au thickness.
ENEPIG Electroless Ni / Electroless Pd / Immersion Au Mixed assembly, soldering and selected bonding Retains a nickel barrier; it is not nickel-free.
EPIG Electroless Palladium Immersion Gold Nickel-sensitive, RF and wire bonding Nickel-free Pd/Au. KKPCB: Pd 1–5 µin; Au 1–5 µin.
ISIG Immersion Silver followed by Immersion Gold Selected RF, fine-pitch and bonding Application-specific review and stack definition required.
Electrolytic Hard Gold Electroplated hard Au Gold fingers and wear-resistant contacts Specify contact zone, Ni underplate, thickness and beveling.
Electrolytic Soft Gold Electroplated soft Au Wire bonding and high-reliability interconnects Review bond method, pad geometry and contamination control.
Electrolytic Nickel / Gold Electroplated Ni/Au Special contact and functional regions Confirm hard, soft, flash or selective gold.
Electrolytic Gold Plating Electrolytic Au Specified special gold layers Define purity, hardness, area and thickness.
Electrolytic Silver Electroplated Ag Special conductive regions Define deposit and tarnish controls.
Electrolytic Tin / Tin-Lead Sn / SnPb plating Special solderable or legacy requirements Do not confuse electrolytic tin with immersion tin.
Selective Gold / Selective ENIG Local or mixed finish One PCB with solderable and wear areas Define masking, process sequence and treated zones.
Carbon Ink / Silver Paste Functional conductive coating Keypads, switches and special conductive features Define resistance, geometry, adhesion, curing and wear.

Terminology: ENIG and Electroless Nickel Immersion Gold describe the same basic process. “Ni/Au”, “immersion gold”, “flash gold” and “selective gold” are not complete specifications by themselves.

PCB fabrication at KKPCB follows IPC Class 2 and Class 3 acceptance criteria (IPC-6012, IPC-A-600) published by IPC.

Layer structures and thicknesses

Source overview reference: chemistry, layers and process behavior

The following engineering starting points are consolidated from the supplied surface-finish overview. Final stack and thickness must be confirmed on the approved fabrication drawing.

Designation Layer structure / reference thickness Process note Relative cost reference
ASIG Ag 0.2–0.4 µm; Au 0.04–0.1 µm Electroless silver / immersion gold; reductive silver route noted as unstable and replaced by ISIG. 140%
ENAG Ni 3–7 µm; Au 0.1–0.3 µm Electroless nickel / electroless gold; reductive gold bath noted as unstable. 120%
ENEPIG Ni 3–7 µm; Pd 0.05–0.3 µm; Au 0.05–0.125 µm Phosphorous Ni and Pd; higher Au thickness possible with semireductive Au deposition. 100%
ENIG Ni 3–7 µm; Au 0.04–0.1 µm Phosphorous nickel with immersion gold; common flat solderable finish. 115%
ENIPIG Ni 3–7 µm; Pd 0.01–0.05 µm; Au 0.04–0.1 µm Nickel / immersion palladium / immersion gold. 90%
EP Pd 0.1–0.2 µm Electroless palladium; palladium without phosphorus. 125%
EPAG Pd 0.1–0.2 µm; Au 0.1–0.2 µm Electroless palladium / electroless gold; nickel-free system. 125%
EPIG Pd 0.1–0.2 µm; Au 0.04–0.15 µm reference Electroless palladium / semireductive gold; KKPCB confirmed Pd 1–5 µin and Au 1–5 µin capability. Review
GalvNiG hard Ni >4 µm; Au 0.8–3 µm Hard gold; Ni hardness 400–450 HV, Au hardness 140–170 HV. >200%
GalvNiG soft Ni >4 µm; Au 0.2–0.5 µm Fine-gold electrolytes for bonding and soldering; Au hardness 80–110 HV. 70%
LF-HASL SnCuNi alloy 1–50 µm Often denoted as HASL; lead-free solderable surface. 70%
Leaded HASL SnPb alloy 1–50 µm Often denoted as HASL; destination-market and regulatory review required. 50%
Immersion Silver Ag 0.2–0.4 µm Flat solderable finish; handling and sulfur control are important. 125%
ISIG Ag 0.2–0.3 µm; Au reference Immersion silver followed by immersion gold. 60%
Immersion Tin Sn 0.8–1.3 µm Planar pure-tin finish; oxidation and storage window require control. 30%
OSP Organic coating 0.2–0.6 µm Organic surface passivation; flat and economical. 1–2x refreshable reference

Primary PDF reference

Surface Finish Overview — complete source matrix

This matrix reproduces the full comparison structure from the supplied Surface Finish Overview PDF: 16 finish designations, layer structures, remarks, soldering and bonding behavior, fine-pitch and RF suitability, press-fit and key-press suitability, corrosion resistance, shelf life, refreshability, market-cost references and example chemistry suppliers. It is a reference map for engineering review; the released drawing and KKPCB feasibility confirmation remain controlling.

▲ Recommended▲ Good with limitations■ With limitations▼ Not recommended▼ Unsuitable
PDF field ASIG ENAG ENEPIG ENIG ENIPIG EP EPAG EPIG GalvNiG hard GalvNiG soft HAL lead free HAL lead containing IS ISIG IT OSP
Description (CONt.) Electroless Silver / Immersion Gold Electroless Nickel / Electroless Gold Electroless Nickel / Electroless Palladium / Immersion Gold Reductive Nickel / Immersion Gold Electroless Nickel / Immersion Palladium / Immersion Gold Electroless Palladium Electroless Palladium / Electroless Gold Electroless Palladium / semireductive Gold HAL HAL lead containing Immersion Silver Immersion Silver / Immersion Gold Immersion Tin OSP
Remarks Semireductive Gold bath. The reductive silver bath has proven too unstable and was replaced by ISIG. Phosphorous Ni. The reductive Au bath is very unstable and is increasingly replaced by Pd-containing alternatives. Phosphorous Ni and Pd; higher Au thickness is possible via semireductive Au deposition (Umicore). Phosphorous Ni. Phosphorous Ni and Pd; higher Au thickness is possible via semireductive Au deposition (Umicore). Pd without phosphorus. Pd without phosphorus; Umicore uses a semireductive TRG gold bath. Pd without phosphorus. Co- or Fe-doped gold baths; Ni hardness 400–450 HV, Au hardness 140–170 HV. Fine-gold electrolytes for bonding and soldering; Ni hardness 400–450 HV, Au hardness 80–110 HV. Often denoted as HASL. Often denoted as HASL. Semireductive gold bath. Organic surface passivation.
Layer type and thickness — Ni 3–7 µm; Au 0.1–0.3 µm Ni 3–7 µm; Pd 0.05–0.3 µm; Au 0.05–0.125 µm Ni 3–7 µm; Au 0.04–0.1 µm Ni 3–7 µm; Pd 0.01–0.05 µm; Au 0.04–0.1 µm Pd 0.1–0.2 µm Pd 0.1–0.2 µm; Au 0.1–0.2 µm Pd 0.1–0.2 µm; Au 0.04–0.15 µm Ni >4 µm; Au 0.8–3 µm Ni >4 µm; Au 0.2–0.5 µm SnCuNi alloy 1–50 µm SnPb alloy 1–50 µm Ag 0.2–0.4 µm Ag 0.2–0.3 µm Sn 0.8–1.3 µm Coating 0.2–0.6 µm
Soldering — ▲ Good ▲ Recommended ▲ Good ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ■ With limitations ▲ Good ▲ Good ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ▲ Good
Multiple solderability — 2× 3× 3× 3× 3× 3× no no no 3× 3× 3× 3× 3× 1–2×
Bonding Al-wire — ▲ Recommended ▲ Recommended ▲ Recommended ▲ Good ▼ Unsuitable ▲ Recommended ▲ Recommended ▼ Unsuitable ▲ Good ▼ Unsuitable ▼ Unsuitable ▲ Recommended ▲ Recommended ▼ Unsuitable ▼ Unsuitable
Bonding Au-wire — ▲ Recommended ▲ Recommended ▼ Not recommended ▲ Good ▼ Unsuitable ▲ Recommended ▲ Recommended ▼ Unsuitable ▲ Recommended ▼ Unsuitable ▼ Unsuitable ▼ Not recommended ▲ Recommended ▼ Not recommended ▼ Not recommended
Fine pitch (pad distance <75 µm) — ■ With limitations ■ With limitations ■ With limitations ■ With limitations ■ With limitations ▲ Recommended ▲ Recommended ▼ Unsuitable ▼ Unsuitable ▼ Unsuitable ▼ Unsuitable ▲ Recommended ▲ Recommended ■ With limitations ▲ Recommended
High frequency application — ■ With limitations ■ With limitations ■ With limitations ■ With limitations ▲ Recommended ▲ Recommended ▲ Recommended ■ With limitations ■ With limitations ■ With limitations ■ With limitations ▲ Recommended ▲ Recommended ■ With limitations ▲ Recommended
Pressfit — ■ With limitations ■ With limitations ■ With limitations ■ With limitations ▲ Good ▲ Good ▲ Good ■ With limitations ■ With limitations ▲ Recommended ▲ Recommended ■ With limitations ■ With limitations ▲ Recommended ▼ Unsuitable
Key press — ▲ Recommended ▲ Recommended ▲ Good ▲ Recommended ■ With limitations ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ▼ Unsuitable ▼ Unsuitable ▼ Unsuitable ▼ Unsuitable ▼ Unsuitable ■ With limitations
Corrosion resistance — ▲ Good ■ With limitations ▲ Good ▲ Good ■ With limitations ▲ Good ▲ Good ▲ Recommended ▲ Recommended ▼ Not recommended ▼ Not recommended ▼ Not recommended ■ With limitations ▲ Good ■ With limitations
Shelf life — ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ▲ Good ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ▲ Recommended ■ With limitations ▲ Recommended ■ With limitations ■ With limitations
Refreshable — no no no no no no no no no yes yes no no yes yes
Long term / market references ■ ▲ ■ ▲ ■ ▼ ▼ ▼ ▲ ▲ ▲ ▲ ▲ ■ ▲ ▲
Serial costs — 140% 120% 100% 115% 90% 125% 125% not specified (local spots) &gt;200% 70% 70% 50% 125% 60% 30%
Chemistry suppliers (inter alia) Umicore Atotech OMG OMG Atotech (Pallabond) Atotech (Pallabond) Umicore (TRG) Dow Dow Balver Zinn Balver Zinn Felder Lote Felder Lote MacDermid Umicore (TRG) Atotech (Smarttin) / Enthone (Entek+ HT)

Note: the source PDF uses colored symbols as a comparative guide. Blank cells mean that the source does not provide a rating for that combination. Cost figures are relative references, not KKPCB quotations.

KKPCB process capability

Released capability references for engineering review

These values are starting points extracted from the available KKPCB capability references. Final feasibility depends on board size, stack-up, copper weight, pad geometry, selected finish and approved fabrication drawing.

EPIG

Nickel-free palladium gold

Pd 1–5 µin · Au 1–5 µin. Each is approximately 0.025–0.127 µm.

ENIG

Electroless nickel immersion gold

Ni 3–6 µm · Au 1–5 µin reference. Flat solderable surface for BGA, QFN and fine pitch.

ENEPIG

Nickel / palladium / gold

Ni 3–5 µm · Pd 1–6 µin · Au 1–4 µin. Retains nickel and supports mixed assembly and selected bonding.

FUNCTIONAL

Carbon ink

10–50 µm prototype reference. Define resistance, geometry, adhesion, curing and wear.

IMMERSION SILVER

Ag 6–12 µin reference

Flat solderable surface for fine pitch and selected high-frequency applications.

IMMERSION TIN

Sn ≥1 µm reference

Lead-free and planar; storage and oxidation controls must be defined.

HARD GOLD

Gold fingers

2–80 µin prototype reference. Confirm beveling, underplate and mating cycles.

SIZE LIMITS

Finish-specific review

ENIG up to 520×800 mm; HASL up to 520×650 mm; hard gold up to 450×500 mm, subject to engineering review.

Process control and handling

From clean copper to a protected interface

Surface-finish quality depends on the full chain: copper preparation, controlled deposition, rinsing, drying, inspection, packaging, storage and assembly discipline.

01 / PREPAREClean & micro-etchRemove oils, oxides and residues to create a uniform copper surface.
02 / DEPOSITBuild the stackDeposit Ni, Pd, Au, Ag, Sn or OSP in the defined sequence.
03 / VERIFYInspect thicknessCheck coverage, solderability, contact areas and drawing requirements.
04 / PROTECTPack & storeUse controlled handling, approved packaging and storage conditions.

OSP · ENTEK PLUS HT reference

Flat co-planar surface compatible with lead-free, mixed-technology, no-clean, air-reflow and press-fit assembly. OSP is economical and flat, but storage duration and multiple thermal cycles require review.

Immersion tin · CSN classic reference

Pure tin is deposited by a metal-replacement reaction at approximately 1 µm. The supplied material notes planar SMD surfaces, multiple soldering cycles, lead-free compatibility, press-fit and fine-pitch use, with proper thickness and storage control.

CleanerRinseMicroetchPredipImmersion TinWarm RinseDI RinseDry

Immersion silver · Sterling reference

Supports strong solder joints, touchpad functionality, wire bondability, low contact resistance and ultra-high RF conductivity. The reference also notes blind-microvia plating for complex boards.

Silver handling and storage

  • Use clean, dry gloves before and after silver processing.
  • Keep boards below 30°C and 75% RH during staging and QC.
  • Use sulfur-free paper and sealed bags; keep air exposure low.
  • Do not use sulfur-bearing tape, labels, ink marks or rubber bands.
  • Do not let plastic wrap or desiccant contact silver surfaces directly.

Design and process review

Via treatment is defined separately from surface finish

Via covering, opening and plugging must follow fabrication data and purchase requirements. A surface finish name does not define whether a via is exposed, tented, filled or plugged.

Design definition

  • State whether vias are exposed, covered, tented, filled or plugged.
  • When plugging and an opening are both required, specify both clearly.
  • For BGA regions, define the via treatment and pad relationship.
  • Avoid ambiguous “according to design files” wording.

Engineering review rules

  • Conflicting or partly exposed definitions require review before fabrication.
  • Via diameters outside validated plugging capability need confirmation.
  • Different treatments on opposite sides can affect appearance and solderability.
  • Final acceptance follows the drawing and agreed inspection criteria.

Industry applications

Surface finishes matched to board function

Use the application as the starting point, then confirm the finish against assembly, environment, reliability target and cost window.

Industrial control

ENIG, lead-free HASL and selective hard gold for durable control, connector and power electronics.

Automotive electronics

ENIG, ENEPIG and selective gold systems for dense assemblies and reliable contacts.

Renewable energy

Lead-free HASL, ENIG and selective contact finishes for inverters, BMS and energy-control hardware.

Medical electronics

ENIG, ENEPIG and application-specific gold for fine pitch, cleanability and high reliability.

RF & high frequency

Immersion silver, EPIG and reviewed stacks for controlled signal surfaces and RF modules.

Consumer electronics

OSP, ENIG and lead-free HASL for compact, fine-pitch and cost-sensitive products.

RFQ ready

What should be confirmed before quotation?

Surface finish selection affects solderability, contact life, storage, compliance, appearance and total cost. A complete RFQ lets engineering quote the correct process without assumptions or rework.

01

Finish system and deposition method

Name the finish and state whether it is chemical, immersion, electrolytic or a mixed/selective process. “Gold” or “Ni/Au” alone is not enough.

02

Metal thickness targets

Specify target and tolerance for nickel, palladium, gold, silver, tin or OSP. Separate the drawing requirement from the engineering reference range.

03

Full-board or selective areas

Identify solder pads, gold fingers, connector contacts, wire-bond pads, carbon contacts and mixed-finish zones. Add masking and sequence notes.

04

Assembly and reliability conditions

Provide lead-free or leaded assembly, reflow cycles, BGA or fine-pitch details, press-fit use, wire-bond method, mating cycles and storage life.

05

Compliance and environment

Confirm RoHS, market restrictions, corrosion exposure, sulfur sensitivity, cleanliness requirements and whether legacy leaded processes are permitted.

06

Drawing and via treatment

Define beveling, via covering/opening/plugging, pad geometry, inspection criteria and any special acceptance notes on the released fabrication data.

Is ENIG suitable for BGA components?

Yes. ENIG provides a flat pad surface and is commonly selected for BGA, QFN and fine-pitch SMT when nickel/gold thickness, solderability and process controls are suitable.

What is the difference between ENIG and hard gold?

ENIG is a chemical nickel/immersion-gold solderable finish. Hard gold is electrolytic, thicker and wear-resistant, normally used for gold fingers, connectors and repeated mating.

What is nickel-free palladium gold?

EPIG is Electroless Palladium Immersion Gold without a nickel barrier. KKPCB confirmed a reviewed capability reference of Pd 1–5 µin and Au 1–5 µin.

Can two finishes be used on one PCB?

Yes. Selective combinations such as ENIG plus local hard gold can separate solderable pads from wear-resistant contacts when zones, masking and process order are defined.

Source file data

Reference terminology and supplier notes

The supplied overview also records the following abbreviations, process descriptions and reference notes. It is retained here for engineering traceability; final production decisions remain drawing- and capability-dependent.

Full source overview notes
recommended / good with limitations / not recommended / unsuitable
Abbreviated designation: ASIG · ENAG · ENEPIG · ENIG · ENIPIG · EP · EPAG · EPIG · GalvNiG hard · GalvNiG soft · HAL lead free · HAL lead containing · IS · ISIG · IT · OSP
Electroless Silver / Immersion Gold · Electroless Nickel / Electroless Gold · Electroless Nickel / Electroless Palladium / Immersion Gold · Reductive Nickel / Immersion Gold · Electroless Nickel / Immersion Palladium / Immersion Gold · Electroless Palladium · Electroless Palladium / Electroless Gold · Electroless Palladium / semireductive Gold · HAL · HAL lead containing · Immersion Silver · Immersion Silver / Immersion Gold · Immersion Tin · OSP
Remarks include: reductive silver bath proven too unstable and replaced by ISIG; reductive Au bath increasingly replaced by Pd-containing alternatives; higher Au thickness possible via semireductive Au deposition; Pd without phosphorus; Co- or Fe-doped gold baths; hard gold Ni hardness 400–450 HV and Au hardness 140–170 HV; soft-gold Au hardness 80–110 HV; often denoted as HASL; semireductive gold bath; organic surface passivation.
Reference layers: Ni 3–7 µm; Pd 0.01–0.3 µm depending on system; Ni >4 µm for electrolytic gold; SnCuNi alloy 1–50 µm; SnPb alloy 1–50 µm; Ag 0.2–0.4 µm; Ag 0.2–0.3 µm; Sn 0.8–1.3 µm; OSP coating 0.2–0.6 µm.
Multiple solderability references in the source include 2x, 3x, 1–2x and “no” depending on finish. Relative serial-cost references include 140%, 120%, 100%, 115%, 90%, 125%, 125%, not specified for local spots, over 200%, 70%, 70%, 50%, 125%, 60% and 30%.
Example chemistry suppliers listed in the source include Umicore, Atotech, OMG, Dow, Balver Zinn, MacDermid, Enthone / Entek+ HT and Felder Lote. These are reference names from the supplied overview, not a statement of KKPCB procurement.

Engineering support

Need help selecting a PCB surface finish?

Send your Gerber files, stack-up, application, assembly process, finish thickness and reliability targets. KKPCB will recommend a practical finish and confirm the process before production.

Upload Gerber Files / Request a Quote